Hostacom ERC 487N G62950 is a 5% talc filled PP copolymer, with excellent flowability, high stiffness, high dimensional stability and excellent scratch resistance. It has been designed using the latest advancements in resin synthesis and compounding technology. Applications: Interior TrimsInformation provided by LyondellBasell. |