MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound ZX06323 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: LNP THERMOCOMP ZX06323 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing proprietary fillers. Added features of this grade include: High Dielectric Constant and Low Loss Tangent

Features: Dielectrics,Circuit Solution

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.95 g/ccASTM D792
 1.95 g/ccISO 1183
Moisture Absorption 0.100 %23°C/50% RH/24 hrs; ASTM D570
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0064 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0056 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPa5 mm/min; ASTM D638
 54.0 MPa5 mm/min; ISO 527
Elongation at Break 4.2 %5 mm/min; ASTM D638
 4.7 %5 mm/min; ISO 527
Tensile Modulus 4080 MPa1 mm/min; ISO 527
 4140 MPa5 mm/min; ASTM D638
Flexural Strength 102 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 102 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3940 MPa1.3 mm/min, 50 mm span; ASTM D790
 4390 MPa2 mm/min; ISO 178
Izod Impact Notched 46.0 JASTM D256
Izod Impact, Unnotched 294 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.4
@Frequency 9.00e+8 Hz
ASTM D2520 - Mth B
Dissipation Factor 0.0030
@Frequency 9.00e+8 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 122 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 295 °C
Zone 2 290 - 295 °C
Zone 3 300 - 305 °C
Melt Temperature 295 - 305 °CInjection Molding
Mold Temperature 90.0 °C
Drying Temperature 105 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Back Pressure 9.00 MPa
Screw Speed 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81990 / 289937

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.