MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODISOLV® RPDE Solvent
Categories: Fluid; Solvent

Material Notes: Rhodiasolv RPDE is an environment friendly, biodegradable, non toxic, non ecotoxic, low VOC solvent.

Identification: DIMETHYL GLUTARATE, DIMETHYL SUCCINATE, DIMETHYL ADIPATE

CAS: 627 – 93 – 0 / 1119 – 40 – 0 / 106 – 65 – 0

CH3COO – (CH2)n – COOCH3 (n = 2, 3, 4)

Available in: Asia Pacific, Europe, Latin America and North America

Solubility: water in solvent: 3.44 and Solvent in water 5.70%

Applications: Paints (can and coil coating), Printing inks, Foundry core binder, Solvent base cleaners, Plasticizer and Magnet wire

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/cc
Viscosity 2.9 cPDynamic
Molecular Weight 158.6 g/mol
Vapor Pressure <= 0.0450 torr
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.30[mg KOH/g], Acidemetry; 540MA3C21
 
Thermal PropertiesOriginal ValueComments
Melting Point -20.0 °CFreezing Point
Distillation Temperature 200 - 235 °C
Flash Point 100 °CClosed Cup; ISO 1523
Ignition Temperature 360 °CAutoignition
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4225
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %540MO3C11
Shelf Life 24.0 Month
 
Descriptive Properties
Color<10APHA, 540MA3C1D
CompositionEster>99.5%, 522MC3C01
 Methanol<0.2% , 540MA3C3A
DistributionDimethyl adipate8-22%, 522MC3C01
 Dimethyl glutarate57-67%, 522MC3C01
 Dimethyl succinate18-28%, 522MC3C01

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAFAC® RS-610 Surfactant
Solvay RHODISOLV® PORLARCLEAN Solvent
Solvay SOPROPHOR® TS/16 Surfactant
Solvay SOPROPHOR® TS/10 Surfactant
Solvay SOPROPHOR® CY/8 Surfactant

WRHOD468 / 137699

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.