MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Marco Polo MarPol IV 80 WB PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PET MarPol IV 80 WB is designed and engineered to provide high dimensional strength and mechanical properties. The low crystallinity and heat of fusion of the resin, provides unique advantages of low residual acetaldehyde generation in injection molding and also lower energy for conversion into bottles. The spherical pellets of the resin ensures smooth conveying in long pipelines with near zero fines generation. The uniform spherical surface allows for easy flow of air around the PET pellets and helps in consistent drying at lower temperatures, saving valuable energy.

Features:

  • Good processability
  • Excellent clarity/gloss
  • Properties balanced for wide range of general purpose usages.
Applications:
  • Various foods, beverages, water etc.
  • Containers for FMCG such as cosmetics, hair-oil, disinfectants
  • Pharmaceuticals
  • APET sheet and PET strapping
Certifications: PET MarPol IV 80 WB resin is considered safe for food-packaging applications based on compliance with US FDA regulation 21 CFR Section 177.1630 & other similar food contact safety regulations

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Test 0.78 - 0.82 dl/gQAF-PCL-3.414
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 1.00 ppmQAF-PCL-3.413
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 - 249 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %when packed
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Color<0.5 bCIE LAB, QAF-PCL-3.211
 >82 LCIE LAB, QAF-PCL-3.211
Properties<100 ppmFine Particles, QAF-PCL-3.407
 1.4-1.8 gmWeight of 100 pcs chips, QAF-PCL-3.408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO079 / 283676

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.