MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
HB Fuller 1581 Silicone system
Categories: Polymer; Thermoset; Silicone

Material Notes: 1581 is a one-component alcohol cure RTV silicone sealant. A non-sag material with excellent heat resistance for use in industrial and electronics applications. 1581 has very good adhesion to a wide range of unprimed substrates. High performance with fast and excellent adhesion to glass, aluminum alloy etc. It can be used for a variety of electronics bonding, encapsulation and sealing applications. This material is certified by UL to pass HB flame rating testing. This material performs at temperatures ranging from -55°C to 210°C.

Features and Benefits:

  • Excellent heat resistance properties
  • Super resistance to ultra violet(UV) and weather
  • Excellent performance in insulation, thermal cycling, damp-heat, damp-freezing
  • Wide operating temperature range
  • Easy to use for reworkable applications
  • Alcohol cure low/no odor
  • RoHS compliant
  • Halogen free
Typical Applications:
  • Electrical insulation
  • Protects leads from mechanical shock
  • Electronics encapsulation
  • Sealing the solar cell side frames
  • Sealing/adhesive solar cell junction boxes
  • Sealing solar energy lamps
  • Sealing and waterproofing for transformer

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/cc
Storage Temperature 8.00 - 25.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 37ISO 7619
Tensile Strength 2.10 MPaISO 37
 1.30 MPa
@Temperature <=85.0 °C,
Time 3.60e+6 sec
Damp Heat Aging Testing; 85% RH; ISO 37
Elongation at Break 380 %ISO 37
 300 %
@Temperature <=85.0 °C,
Time 3.60e+6 sec
Damp Heat Aging Testing; 85% RH; ISO 37
Shear Strength 1.20 MPaLap Joint, Aluminum; ISO 4587
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+15 ohm-cmIEC 60093
Dielectric Strength 20.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 minTack Free
 24.0 hour
@Thickness >=2.00 mm
Full-cure
 
Descriptive Properties
ColorWhite
ConsistencyThixotropic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL098 / 316889

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.