MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC)

Material Notes: Acrylonitrile Styrene Acrylate + Polycarbonate

Preliminary Data
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 8.0 - 18 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7500 psiASTM D638
Tensile Strength, Yield 8500 psiASTM D638
Flexural Strength 11000 psiASTM D790
Flexural Modulus 377 ksiASTM D790
Izod Impact, Notched 4.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 215 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 470 °F
Middle Barrel Temperature 470 - 490 °F
Front Barrel Temperature 490 - 520 °F
Melt Temperature 490 - 520 °F
Mold Temperature 130 - 160 °F
Drying Temperature 190 - 210 °F
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB SCANBLEND FS8 ASUV4 PC/ASA, Antistatic, Improved Weather Resistance
Covestro Bayblend® FR3010 HF PC/ABS Blend
Polykemi AB SCANBLEND FS7 UV4 PC/ASA Blend with Improved Weather Resistance
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
INEOS Styrolution Novodur® HH-112 ABS

PPOLYQ194a / 160715

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.