MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C17510, TF00 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Spot Weld, Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Seam Weld, Butt Weld

Common Fabrication Processes: Blanking, Drilling, Forming and Bending, Tapping, Turning

Typical Uses: Conductors; Connectors, Heavy Duty; Fuse Clips; Instrument Parts; Relay Parts; Switch Parts; Fasteners; Die casting plunger tips; High Flux Electromagnets; Springs; Thermal Transfer Plates; Welding Equipment

Applicable Specifications: Bar - ASTM B441; ASTM B534; Forgings & Extrusions – ASTM B870; Heat Exchanger Tube – ASTM B944; Plate – ASTM B534; Rod – SAE J463, ASTM B441, SAE J461; Seamless Tube – ASTM B937; Shapes – SAE J463, SAE J461; Sheet – ASTM B534; Strip – SAE J461, ASTM B888/B88M, SAE J463, MILITARY MIL-C-81021, ASTM B534; Tube – SAE J463, SAE J461

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.317 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 96
Tensile Strength 110 ksi
Tensile Strength, Yield 90.0 ksi0.5% Ext
Elongation at Break 18 %
Tensile Modulus 19200 ksi
Modulus of Rigidity 7500 ksi
Poissons Ratio 0.28Calculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000360 ohm-cm48% IACS; Cold worked and precipitation hardened condition. HT Temper
 0.00000380 ohm-cm45% IACS; AT Temper
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.100 BTU/lb-°F
Thermal Conductivity 120 BTU-in/hr-ft²-°F
Melting Point 1885 - 1955 °F
Solidus 1885 °F
Liquidus 1955 °F
 
Processing PropertiesOriginal ValueComments
Solution Temperature 1550 - 1700 °F
@Time 60.0 sec
Water
Hot-Working Temperature 1200 - 1750 °F
Precipitation Temperature >= 850 °FAir
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.20 %
Beryllium, Be 0.20 - 0.60 %
Cobalt, Co <= 0.30 %
Copper, Cu 96.4 - 98.4 %As Balance
Iron, Fe <= 0.10 %
Nickel, Ni 1.4 - 2.2 %
Silicon, Si <= 0.20 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC17510y1 / 291602

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.