MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEMUV-3638 Light Absorber
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS NO. 18600-59-4

GOYENCHEMUV-3638 is a highly-effective UV absorber based on the structure of benzoxazinone that is with high stability and light fastness properties. Thanks to its twice the absorption at UV-A range than triazine or benzotriazole based UV absorbers on the same weight basis, GOYENCHEMUV-3638 is perfectly suitable for engineering plastics and polymers which extra protection at blue-swift UV regions is required.

Features/Benefits:

  • Provides plastics or polymers excellent UV protection
  • High stability and light fastness properties
Applications:
  • Engineering plastics: PET, PBT, etc.
  • Polymers which extra protection at blue-swift UV regions is required

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 369 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 310 °C
 
Descriptive Properties
AppearanceWhite to off-white crystalline powder
AssayHPLC
Loss on drying<0.5%
Solubility<0.01%100ml solvent, Water
 <1%100ml solvent, DMF
 <1%100ml solvent, Ethanol
 <1%100ml solvent, Ethyl acetate
 <1%100ml solvent, Methyl ethyl ketone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN554 / 266862

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.