MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
P & P Technology KE Series Cored Shielding Mesh Gasket Strip
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Cover: Knitted Monel To BS 3075-NA 13 0.11mm Dia 2 Layers.

Core Material: Neoprene closed cell sponge.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.150 - 0.210 g/cc
Water Absorption 0.70 %core
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38 - 55
Compression Set 17 %
@Time 86400 sec
50% compression
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 285 dBTo Mil Stn
 45 dB
@Frequency 10000 Hz
H-Field
 49 dB
@Frequency 100000 Hz
H-Field
 60 dB
@Frequency 1e+6 Hz
H-Field
 75 dB
@Frequency 1e+10 Hz
P-Field
 89 dB
@Frequency 1e+9 Hz
P-Field
 >= 100 dB
@Frequency 1e+6 Hz
E-Field
 >= 100 dB
@Frequency 1e+7 Hz
E-Field
 >= 100 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -38.0 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurofoam Porocell POR 303/B/CM CR-Neoprene/NBR Foam
Denka Neoprene WHV-100 Polychloroprene Rubber
Denka Neoprene GW Polychloroprene
Armacell Monarch® F-05091 (Black) Neoprene, EPDM, SBR Blend Foam
Armacell Monarch® F-03043 (Black) Neoprene Based Rubber Foam

PPPTEC010 / 133474

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.