MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
P & P Technology Polyester Polyurethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: High performance acoustic and dust filtration foam with a density of 60 Kg/cubic meter with excellent fire resistance properties. Used in heating, ventilation, electronic, aeronautic, automotive and computer industries.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.0550 - 0.0650 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 0.120 MPa
Elongation at Break 200 %
Compression Set <= 10 %
@Temperature 70.0 °C,
Time 79200 sec
75% comp
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 110 °C
Minimum Service Temperature, Air -30.0 °C
 
Descriptive Properties
Porosity55-75 pores per inch

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NRI Viper-Skin™ Carbon Fiber Composite
NRI Syntho-plug™
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black
Dow BETAMATE™ 7200 Polyurethane Prepolymer

PPPTEC023 / 133487

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.