Waterborne-based one-coat adhesive for bonding fluorocarbon (both peroxide and bisphenol/diamine cure systems), peroxide cured EPDM, VMQ and some peroxide cured AEM compounds to metals and other solid materials under vulcanization conditions.Information provided by DuPont. |