MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE EE-2275N Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-2275N is a general purpose thermoplastic elastomer designed for automotive exterior applications. Sarlink EE-2275N exhibits good elastic properties with sunlight resistance and UV absorbing characteristics.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; High Density; Low Flow; High Specific Gravity; Light Stabilized; Medium Hardness; Sunlight Resistant; UV Absorbing

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Viscosity 289 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 15.0 sec
Injection Molded; ISO 868
 76
@Time 5.00 sec
Injection Molded; ISO 868
 78
@Time 1.00 sec
Injection Molded; ISO 868
 72.4
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
 73.5
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 75.2
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 75.5
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 76.9
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 78.8
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
Tensile Strength at Break 885 psiFlow, Type 1, 20 in/min; ISO 37
 1260 psiAcross Flow, Type 1, 20 in/min; ISO 37
 856 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 856 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 1200 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 1230 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 351 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 466 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 407 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 168 hr; ISO 188
 411 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 536 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
 536 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
Elongation at Break 580 %Flow, Type 1, 20 in/min; ISO 37
 750 %Across Flow, Type 1, 20 in/min; ISO 37
 537 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 646 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 713 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 732 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 180 pliAcross Flow; ISO 34-1
 200 pliFlow; ISO 34-1
Compression Set 27 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 47 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 70 %
@Temperature 90.0 °C,
Time 252000 sec
Type A; ISO 815
 81 %
@Temperature 125 °C,
Time 252000 sec
Type A; ISO 815
 
Processing PropertiesOriginal ValueComments
Zone 1 380 - 400 °F
Zone 2 390 - 410 °F
Zone 3 400 - 420 °F
Zone 5 410 - 430 °F
Die Temperature 420 - 440 °F
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1036 / 237527

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.