MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Radel® R-7300 Polyphenylsulfone (PPSU), Premium grade
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Premium grade, high flow for injection molding, suitable for light colors, for aircraft interiors

Radel® R-7300 (for light colors) and R-7400 (for darker colors) polyphenylsulfone resins were developed specifically for aircraft interior applications, and through the use of a proprietary flame retardant package, offer low heat release, low smoke generation, and low toxic gas emissions. These resins comply with the FAA regulation 14CFR Part 25.853 Appendix F. In addition, they have excellent impact resistance and ESCR when exposed to fluids typically used by the aerospace industry, reducing the need for annealing or protective films.

Radel® R-7300 and R-7400 resins have excellent flow characteristics, readily filling complex parts with thin walls or long flow lengths.

Chemical Resistance:
One of the outstanding characteristics of Radel® R-7300 and R-7400 resins is their resistance to many commonly used aviation fluids. Three test methods: unstressed immersion, stressed with a 5-inch radius curve, and stressed with a variable radius curve fixture, were employed to evaluate resistance of Radel® resins to Skydrol® LD-4; 1,1,1-trichloroethane; Jet fuel A; methyl ethyl ketone; toluene; isopropanol; and Skydrol® 500B.

- Available in various custom colors

Markets/Uses: Aircraft / Aircraft Interiors / Air Vents and Return Grilles; Aircraft / Aircraft Interiors / Infill Panels; Aircraft / Aircraft Interiors / Oxygen Boxes; Aircraft / Aircraft Interiors / Passenger Service Units; Aircraft / Aircraft Interiors / Video Shrouds; Aircraft / Aircraft Interiors / Window Reveals and Shades

Applications: Aerospace Applications; Aircraft Applications; Aircraft Interiors

Features: Chemical Resistant; Detergent Resistant; Flame Retardant; Good Processing Stability; Good Toughness; High Flow; Low Smoke Emission; Low Toxicity

Materials intended for aircraft interior parts must meet stringent flammability requirements. Radel R-7300 and R-7400 resins meet or exceed all commercial and regulatory requirements for flammability, smoke density, heat release, and toxic gas emissions.

OSU Peak Heat Release Rate - FAR 25.853(d) < 55.0 kW/m²; OSU Total Heat Release - FAR 25.853(d) < 20.0 kW·min/m²; Smoke Density - ASTM F814 < 5.0 Ds; Smoke Density - ASTM F814 1.0 Ds

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
ASTM D570
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.8 MPaASTM D638
Elongation at Break 40 %ASTM D638
Tensile Modulus 2790 MPaASTM D638
Flexural Strength 110 MPaASTM D790
Flexural Modulus 2760 MPaASTM D790
Izod Impact, Notched 80.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 182 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 354 - 371 °C
Middle Barrel Temperature 360 - 377 °C
Front Barrel Temperature 366 - 382 °C
Nozzle Temperature 360 - 377 °C
Melt Temperature 366 - 388 °CInjection
Mold Temperature 107 - 163 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorColors Available
FormsPellets
Injection RateFast
ProcessingInjection Molding
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4401 / 280201

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.