MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 5 Neoprene Contact Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Neoprene Contact Adhesive 5 is a sprayable contact adhesive which may be used to bond many high-pressure plastic laminates to wood, particle-board, metal and other surfaces

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 18 - 21 %
Brookfield Viscosity 175 - 350 cPRVF #2 sp @ 20 rpm @ 80°F
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 38.0 psi
@Temperature 107 °C,
Time 1.81e+6 sec
Overlap
 65.0 psi
@Temperature 82.0 °C,
Time 1.81e+6 sec
Overlap
 480 psi
@Temperature 75.0 °C,
Time 1.21e+6 sec
Overlap
 482 psi
@Temperature 75.0 °C,
Time 1.81e+6 sec
Overlap
 1060 psi
@Temperature -34.0 °C,
Time 1.81e+6 sec
Overlap
Peel Strength 7.00 pli
@Temperature 82.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 10.0 pli
@Temperature 24.0 °C,
Time 86400 sec
180°, Canvas/Steel
 12.0 pli
@Temperature 24.0 °C,
Time 259000 sec
180°, Canvas/Steel
 14.0 pli
@Temperature 24.0 °C,
Time 432000 sec
180°, Canvas/Steel
 16.5 pli
@Temperature -34.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 18.0 pli
@Temperature 24.0 °C,
Time 605000 sec
180°, Canvas/Steel
 18.0 pli
@Temperature 24.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
 19.0 pli
@Temperature 24.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 
Thermal PropertiesOriginal ValueComments
Flash Point -25.0 °CTCC
 
Descriptive Properties
AppearanceGreen, Light Yellow
BasePolychloroprene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 10 Neoprene Contact Adhesive
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives

PMM34111 / 168858

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.