MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Qualchem Danamid FES-21 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Impact resistant, dry

Information provided by Qualchem Zrt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccDIN 53479
Moisture Absorption at Equilibrium 3.0 - 3.2 %DIN 53714
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527-1,2
Elongation at Yield 10 %ISO 527-1,2
Tensile Modulus 1.60 GPaISO 527-1,2
Charpy Impact Unnotched NB
@Temperature -20.0 °C
DIN 53453
 NB
@Temperature 23.0 °C
DIN 53453
Charpy Impact, Notched >= 0.500 J/cm²
@Temperature -20.0 °C
DIN 53453
 >= 1.20 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN 53482
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 4.00 mm
MSZ 10383

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 216 PA66, Conditioned
Overview of materials for Nylon 66, Heat Stabilized
Evonik TROGAMID® CX9710 Polyamide
Evonik TROGAMID® CareMX7-L Polyamide
Envalior Stanyl® TE351 PA46 FR(17)

PQUALC23 / 58435

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.