Description: Sheet Extrusion or Injection Molding, PC/ABS+CNT, Electrostatic Dissipation, Wide Processing Range, Low Surface Resistivity Application: BLU Carrying Tray CAS No. 103598-77-2, 9003-56-9, 1333-86-4 and 7782-42-5 Information provided by LG Chemical |