MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any starch or starch derivatives. Bioplastics generally replace conventional materials such as low density polyethylene (LDPE), high density polythene (HDPE) as well as polystyrene (PS) and polypropylene (PP). For packaging applications these materials need to be converted into film which is as thin as possible while maintaining high tensile strength. Depending on the specific application, packaging films have to provide a high barrier against humidity, oxygen and aromas or alternatively provide adequate permeability (“breathability”).

BIO-FLEX® S 9533 has been designed especially for injection moulding applications. Ideal for moulding, a result of its excellent flow characteristics, its mechanical properties are comparable to conventional polystyrene (PS). Furthermore BIO-FLEX® S 9533 is biodegradable with a high percentage of renewable resource raw material content.

Information Provided by FKuR Kunststoff GmbH
Key Words: Polylactic Acid; biodegradable film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccISO 1183
Melt Flow 12 - 14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.0 MPaISO 527
Elongation at Break 5.0 %ISO 527
Elongation at Yield 3.8 %ISO 527
Tensile Modulus 4560 MPaISO 527
Flexural Modulus 4680 MPaISO 178
Flexural Strain at Break 2.9 %ISO 178
Charpy Impact Unnotched 27.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eU
Charpy Impact, Notched 1.50 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 150 - 170 °CISO 3146-C
Vicat Softening Point 63.0 °CA; ISO 306
 
Descriptive Properties
Tensile stress at break (MPa)43ISO 527

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend

PFKUR006b / 138487

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.