MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DF002FVQ Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DF002FVQ compound is based on Polycarbonate (PC) resin containing 10% glass fiber and available in black color only. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Good Adhesion Strength, UL94 V0@0.8mm (black).

Features: High Stiffness,Good metal adhesion,Laser Direct Structuring,Circuit Solution

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cmSABIC method
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa5 mm/min; ASTM D638
 60.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ASTM D638
 3.5 %5 mm/min; ISO 527
Tensile Modulus 4610 MPa5 mm/min; ASTM D638
 4625 MPa1 mm/min; ISO 527
Flexural Strength 110 MPa2 mm/min; ISO 178
 115 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4100 MPa2 mm/min; ISO 178
 4300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 100 JASTM D256
Izod Impact, Unnotched 600 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Charpy Impact Unnotched 42.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.04
@Frequency 2.00e+10 Hz
SABIC method
 3.15
@Frequency 1.10e+9 Hz
SABIC method
 3.15
@Frequency 5.00e+9 Hz
SABIC method
 3.17
@Frequency 1.90e+9 Hz
SABIC method
 3.17
@Frequency 1e+10 Hz
SABIC method
Dissipation Factor 0.010
@Frequency 1.10e+9 Hz
SABIC method
 0.010
@Frequency 1.90e+9 Hz
SABIC method
 0.010
@Frequency 5.00e+9 Hz
SABIC method
 0.010
@Frequency 1e+10 Hz
SABIC method
 0.010
@Frequency 2.00e+10 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 35.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.800 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 285 - 310 °C
Zone 2 285 - 310 °C
Zone 3 285 - 310 °C
Melt Temperature 290 - 310 °CInjection Molding
Mold Temperature 100 - 130 °C
Drying Temperature 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa
Screw Speed 50 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81508 / 289455

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.