Data provided by the manufacturer, Exxon Chemical. A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability. Applications: Primal meat bags; Retail meat packages; Cheese packaging. Data for film properties below based on 1.25 mil film. |
Ethylene Vinyl Acetate; Exxon Chemical Company |