MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® L1930 black 9.7506 Nylon 12, 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 30% Glass Fiber Filled

Material Notes: VESTAMID® L1930 black 9.7506 is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding. Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity. Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 black 9.7506 the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded. As a semi-crystalline material VESTAMID® L1930 black 9.7506 feature an outstanding chemical resistance, e.g., against fuels, oils and fats. VESTAMID® L1930 black 9.7506 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccISO 1183
Water Absorption 1.1 %Sim. to ISO 62
Moisture Absorption 0.500 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527
Tensile Strength 64.0 MPaISO 527
Tensile Strength, Yield 64.0 MPaISO 527
Elongation at Break 12 %Nominal; ISO 527
Elongation at Yield 4.0 %ISO 527
Tensile Modulus 3800 MPaISO 527
Charpy Impact Unnotched 65.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 170 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75-1/-2
Vicat Softening Point 170 °CMethod B: 10 N, 50 K/h; ISO 306
 175 °CMethod A: 10 N, 50 K/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CTest condition for mold shrinkage
Mold Temperature 80.0 °CTest condition for mold shrinkage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK849 / 243057

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.