(Viewing data as-entered.
Click here
to return)
ATI Allegheny Ludlum A6 Tool Steel, UNS T30106
Categories:
Metal
;
Ferrous Metal
;
Tool Steel
;
Air-Hardening Steel
;
Cold Work Steel
Material Notes:
An air hardening cold work grade with superior nondeforming properties. Particularly attractive for dies, punches, gages and other tools where close size tolerance is important.
Information provided by Allegheny Ludlum
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.03
g/cc
Based on UNS number
Component Elements Properties
Original Value
Comments
Carbon, C
0.70 %
Chromium, Cr
1.0 %
Iron, Fe
95 %
as balance
Manganese, Mn
2.0 %
Molybdenum, Mo
1.3 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AISI Type H22 Tungsten Hot Work Tool Steel (UNS T20822)
Kinetics MIM 4605 Low Alloy Steel (As Sintered)
Assab Steels ASSAB 88 Cold Work Steel
Assab Steels 709M Machinery Steel
AISI Type H24 Tungsten Hot Work Tool Steel (UNS T20824)
NLTA6 / 18047
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.