LNP THERMOCOMP UX06032 compound is based on Polyphthalamide (PPA) resin containing 30% glass fiber. Added features of this grade include: Non-Brominated & Non-Chlorinated Flame Retardant, Heat Stabilized. Features: High Stiffness,Flame Retardant,Non-Chlorinated,Non-Brominated,Heat Stabilized,Structural Information provided by SABIC |