MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röhm CYROLITE® MD H12 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: CYROLITE® MD H12 acrylic polymer is an amorphous thermoplastic molding compound based on polymethyl methacrylate (PMMA) for the medical diagnostic industry.

Typical properties of CYROLITE® MD acrylic polymers are:

  • Exceptional ultra-violet light transmittance
  • Superior optical clarity
  • Maximum flow characteristics
  • Excellent dimensional stability
  • Outstanding scratch resistance
  • Total cost-of-use advantage over glass
The special properties of CYROLITE® MD H12 are:
  • Higher Vicat softening point
  • Medium melt flow rate
Application: Used for injection molding of medical devices requiring UV spectroscopy for fluid evaluation.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Bulk Density 0.660 g/ccASTM D1895
Water Absorption <= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 94ASTM D785
Tensile Strength 65.5 MPaASTM D638
Elongation at Break 4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %ASTM D638
Tensile Modulus 3.20 GPaASTM D638
Flexural Strength 117.2 MPaASTM D790
Flexural Modulus 3.40 GPaASTM D790
Izod Impact, Notched 19.0 J/m
@Thickness 6.35 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 105 °C
@Load 5.10 kg
50°C/h; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Yellow Index <= 1.0 %ASTM D1003
Transmission, Visible 92 %ASTM D1003
UV Transmittance <= 87.7 %
@Wavelength 340 nm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9348 / 319965

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.