MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lanxess Addocat® 9727 P PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 9727 P is a powerful catalyst for the gas reaction. Addocat 9727 P is one of the standard catalysts for polyether flexible foam systems (0.10 - 0.15 p.b.w. Addocat 9727 P on 100 p.b.w. polyether polyol). The crosslinking reaction is catalyzed with Addocat SO (Sn-octoate 0.1 - 0.3 p.b.w.). Addocat 9727 P is a base catalyst which, to enable the reaction to be more carefully controlled, can be combined with mild co-catalysts, without narrowing the Sn-octoate range.

Function: Catalyst for the production of polyurethane foams, e.g. flexible slabstock foam (ether type), hot molded foam, HR foam.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc0.0316 lb/in³
Water Absorption <= 0.50 %<= 0.50 %
Viscosity 3.0 cP3.0 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point -60.0 °C-76.0 °FFreezing Point
Boiling Point 140 °C284 °FInitial
Flash Point 47.0 °C117 °FEN ISO 13736
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 10.0 - 30.0 °C
6.00 Month
@Temperature 50.0 - 86.0 °F
 
Descriptive Properties
Appearanceclear, colorless to slightly yellowish liquid
Content20 percentBasic Nitrogen
Specifications280 mg KOH/gOH-value

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8194 / 208587

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.