MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRES™ SLX2271AML Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES SLX2271AML is based on Polycarbonate (PC) siloxane copolymer resin. It is an antimicrobial compound available in transparent and tinted colors. Added features of this grade include: Good Weatherability and Scratch Resistance.

Features: Scratch Resistance,Weatherable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 22 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 61.3 MPa50 mm/min; ASTM D638
 62.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 61.6 MPa50 mm/min; ISO 527
 61.9 MPa50 mm/min; ASTM D638
Elongation at Break 93 %50 mm/min; ASTM D638
 99.7 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2368 MPa5 mm/min; ASTM D638
 2382 MPa1 mm/min; ISO 527
Flexural Strength 82.3 MPayield, 2 mm/min; ISO 178
 102 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2360 MPa1.3 mm/min, 50 mm span; ASTM D790
 2487 MPa2 mm/min; ISO 178
Izod Impact Notched 119 JASTM D256
 89.5 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 13.5 kJ/m²80*10*3; ISO 180/1A
 9.30 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 13.6 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 9.20 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 66.1 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 140 °CRate B/50; ASTM D1525
 141 °CRate B/120; ISO 306
 141 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 290 °C
Zone 2 270 - 290 °C
Zone 3 280 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80598 / 288545

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.