General Properties: The NP Life Time range consists of a set of biobased and biodegradable polyester-based compounds. The products in this range were specifically designed to accelerate or reduce the rate of biodegradation of the products. Applications: Process: Markets: - Agriculture / horticulture
- Consumption goods
Properties:- Partially to completely biosourced
- Biodegradable and compostable
- Accelerated or slowed degradation depending on the product
Information provided by NaturePlast Bioplastics Experts |