MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Idemitsu Kosan TARFLON NEO™ RC2031 Polycarbonate-PDMS Copolymer
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Siloxane

Material Notes: General information on TARFLON NEO™ PC-PDMS Copolymer (Polydimethylsiloxane): Excellent low-temperature impact ductility at -30°C and below, Superior balance of flow ability and impact strength, Good chemical resistance (Especially good resistant to alkali, compared with standard PC), Long-term stability in physical properties (Especially in weather ability), Good heat-resistance (Same as that of standard PC).

Information provided by Idemitsu Losan Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183(JIS K7112)
Moisture Absorption 0.200 %
@Time 86400 sec
50% RH; ISO 62(JIS K7209)
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
@Thickness 2.00 mm
Idemitsu Method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 2.00 mm
Idemitsu Method
Melt Flow 10.18 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133 (JIS K7210)
Spiral Flow 22.0 cm
@Thickness 2.00 mm
Width:10mm. Cylinder: 240°C/Mold: 40°C. Inj.Pressure: 125 MPa.; Idemitsu Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 59.0 MPaISO 527-1,2 (JIS K7161, 7162)
Elongation at Break 115 %Nominal; ISO 527-1,2 (JIS K7161, 7162)
Flexural Strength 90.0 MPaISO 178 (JIS K7171)
Flexural Modulus 2.20 GPaISO 178 (JIS K7171)
Izod Impact, Notched 700 J/m
@Temperature -30.0 °C
ASTM D256
 800 J/m
@Temperature 0.000 °C
ASTM D256
 820 J/m
@Temperature 23.0 °C
ASTM D256
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1(JIS K7111)
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1(JIS K7111)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°CISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 123 °CISO 75-1,2 (JIS K7191-1,2)
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 87 %Total Luminous; ISO 13468-1 (JIS K7361-1)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 310 °CCylinder Temperature
 <= 320 °CMax Cylinder Temperature
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °C
@Time 18000 - 28800 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PIDEM209 / 249573

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.