MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC PVC 673E Emulsion Polyvinyl Chloride  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product Description: PVC 673E is a fine particle, medium-molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting high viscosity at low shear rates with Newtonian flow characteristics at high shear rates with plasticizer concentrations of 40-60 Phr. Because of the low viscosity of PVC 673E pastes, this resin is recommended primarily for low plasticized applications (hard plastisol application). Plastisols made from this resin exhibit the following main properties:
  • Low gelation temperature
  • Low plastisol viscosity at low shear
  • Low plastisol viscosity at high shear (Newtonian)
  • Ability to form stable plastisol at low levels of plasticizer (100 PVC, 50 DOP)
  • Long shelf life, low viscosity aging
  • Little tendency to sediment
  • Good thermal stability with a range of standard stabilizers

Typical Applications: PVC 673E has been developed for making plastisols of low yield points and low viscosity, agents. PVC 673E plastisols are ideal for chemical foams of very good quality with very regular closed cell structure, over a large range of oven temperatures. The main applications are

  • Cushioned vinyl flooring
  • Artificial leather

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.320 g/ccISO 60
Volatiles <= 0.30 %ISO 1269
Particle Size <= 63 µm1.80% retained; ISO 1624
 <= 106 µm0.05% retained; ISO 1624
Viscosity 5000 cP
@Pressure 0.621 MPa
Servers; ASTM D-1823
Brookfield Viscosity 25000 cP20 rpm; ISO 2555/4575
 
Descriptive Properties
K-Value67ISO 1628-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for 7000 Series Aluminum Alloy
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion
Overview of materials for PVC, Extruded
Overview of materials for PVC, Molded
Overview of materials for PVC, Sheet Grade

PSABICZ898 / 133094

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.