MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3M Scotch® Super 88 Vinyl Electrical Tape
Categories: Polymer; Tape; Thermoplastic; Vinyl (PVC)

Material Notes: Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is conformable for cold weather application down to -18°C. It has excellent resistance to abrasion, moisture, alkalies, acids, corrosion and varying weather conditions. The combination of elastic backing and aggressive adhesive provides moisture-tight electrical and mechanical protection with minimum bulk. It is UL Listed and is a Canadian Standards Association (CSA) Certified “Insulating Tape”.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 216 microns8.50 mil
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break  100 %
@Temperature -18.0 °C
100 %
@Temperature -0.400 °F
ASTM D1000
 250 %
@Temperature 22.0 °C
250 %
@Temperature 71.6 °F
ASTM D1000
Peel Strength  0.307 kN/m
@Temperature 2.00 °C
1.75 pli
@Temperature 35.6 °F
Adhesion to Steel; ASTM D1000
 0.307 kN/m
@Temperature 22.0 °C
1.75 pli
@Temperature 71.6 °F
Adhesion to Backing; ASTM D1000
 0.657 kN/m
@Temperature -18.0 °C
3.75 pli
@Temperature -0.400 °F
Adhesion to Steel; ASTM D1000
 0.657 kN/m
@Temperature -18.0 °C
3.75 pli
@Temperature -0.400 °F
Adhesion to Backing; ASTM D1000
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D1000
Dielectric Breakdown 9000 V9000 VHigh Humidity; ASTM D1000
 10000 V10000 VStandard condition; ASTM D1000
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -18.0 °C-0.400 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35170 / 169917

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.