MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Celanese Hytrel® G4774 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing Protection

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Melt Density 1.01 g/cc
@Temperature 240 °C
Water Absorption 2.5 %
@Time 86400 sec
Immersion; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cmISO 294-4, 2577
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
cm³/10min Volumetric; ISO 1133
 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4315s; ISO 48-4
 <= 48ISO 48-4
Tensile Stress at Strain 7.00 MPa
@Strain 10 %
ISO 527-1/-2
 12.0 MPa
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 111 MPaISO 178
Izod Impact, Notched (ISO) NB
@Temperature -40.0 °C
ISO 180/1A
 NB
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 120 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Tensile Impact Strength 260 kJ/m²
@Temperature 23.0 °C
Notched; ISO 8256/1
Tear Strength 90.0 kN/mnormal; ISO 34-1
 100 kN/mparallel; ISO 34-1
Abrasion 33mm3; ISO 4649
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 220 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 190 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 2.10 J/g-°C
@Temperature 240 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 240 °C
Melt
Melting Point 208 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -66.0 °CISO 974
Glass Transition Temp, Tg -45.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10
Flame Spread 33.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °COptimum, Extrusion
 225 - 240 °CRange, Extrusion
 240 °COptimum, Injection
 235 - 260 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 100 °CInjection
 100 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
Emission of organic compounds (µgC/g)18VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Odor Class5VDA 270
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 4556 TPC-ET
Celanese Hytrel® 4068 TPC-ET
Celanese Hytrel® G5544 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® 8238 TPC-ET

PDSX5200 / 197840

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.