PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PRE-ELEC CP 1316 has good mechanical properties and is easy to extrude or injection mould. Typical applications include flexible extruded profiles and tubes and flexible injection molded parts. PRE-ELEC CP 1316 may also be used as a masterbatch and blended with EVA or PE-LD. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc. |