MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Thermal Ceramics Cease 2000 Fire
Categories: Ceramic

Material Notes: Cease Fire 2000 is a unique, two-component refractory foam. The dry powder (component A) is mixed with water to form a semi-viscous slurry and then combined with mild phosphoric acid (component B) at the pumping nozzle. The reaction produces a foam of approximately 1½ times its original volume. The process involves the generation of moderate heat from which evolves non-toxic gaseous by-products resulting in a network of independent cellular pores. The fast setting time of Cease Fire alleviates the need for extended drying or curing times. Since the reaction is complete, steam spalling on the initial fire is not a concern.

Features:

  • Fluid nature readily fills backup insulation voids
  • Highly insulating foam product (thermal conductivity equivalent to ceramic fiber)
  • Easily installed while unit is on or off-line
  • Unique pore structure allows for controlled crushing instead of catastrophic cracking
  • Suitable for use up to 2000°F (1093°C)
  • Typical Applications:

    Utility boilers:

  • penthouse floors and walls
  • superheater penetration
  • Iron and Steel

  • blast furnace stoves, hot blast mains, and bustle pipes
  • soaking pit sidewalls
  • coke oven backup and seals
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesOriginal ValueComments
    Compressive Yield Strength 0.140 - 0.280 MPa10% Compression
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.600 BTU-in/hr-ft²-°F
    @Temperature 260 °C
     0.750 BTU-in/hr-ft²-°F
    @Temperature 149 °C
     0.800 BTU-in/hr-ft²-°F
    @Temperature 371 °C
     0.900 BTU-in/hr-ft²-°F
    @Temperature 482 °C
     1.00 BTU-in/hr-ft²-°F
    @Temperature 593 °C
    Maximum Service Temperature, Air 2000 °F
    Shrinkage 0.00 %
    @Temperature 104 °C,
    Time 18000 sec
     1.0 - 1.5 %
    @Temperature 538 °C,
    Time 18000 sec
     2.0 - 3.0 %
    @Temperature 1090 °C,
    Time 18000 sec
     
    Processing PropertiesOriginal ValueComments
    Shelf Life 6.00 Month
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 34 %
    CaO 12 %
    Fe2O3 0.80 %
    Other 1.0 %
    SiO2 35 %
    TiO2 1.2 %
     
    Descriptive Properties
    % Volume increase50
    Initial set time, sec60-120
    P2O3 content16%
    Rise time at 70°F, sec30-90
    Slurry/ Acid ratio by volume4:1
    Slurry/ Acid ratio by weight4.5:1

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Pyrotek Mesh core / Z-6W Tadpoles
    Pyrotek Mesh core / V-5 Tadpoles
    Pyrotek Jacketed mesh core Tadpoles
    Pyrotek Bonded Particle Filtration Media
    Johnson Matthey Easy-flo™ 100 Flux Paste Brazing Flux

    CTHERM261 / 2581

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.