EMERGE™ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycarbonate resins.
Applications: - Consumer Electronics
- Information Technology Equipment
- Appliances
Information provided by Dow This product line was spun off from Dow Chemical to Styron in 2010. |