MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Top Polymer Topolymer® 3211 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Production Description: Topolymer® 3211 is an easy processing compound used for wire and cable, which based on SEBS/SEPS of Kraton & Kuraray and Engage/Infuse of Dow. Topolymer® 3211 is valuable in applications for earphone lines, mobile charger lines, etc.

Features: Low Special Gravity, Soft Touch, Easy Processing.

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 - 1.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60 - 99
Tensile Strength >= 65.0 kg(f)/cm²
Tear Strength Test >= 450[%]
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Zone 1 140 - 160 °CExtrusion
Zone 2 160 - 180 °CExtrusion
Zone 3 170 - 200 °CExtrusion
Die Temperature 170 - 200 °CExtrusion
Melt Temperature 170 - 200 °CExtrusion
Head Temperature 170 - 200 °CExtrusion
 
Descriptive Properties
ColorNatural
Compress Ratio3:1Extrusion
Filter100-150 MeshExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOPO002 / 184514

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.