MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

(Viewing data as-entered. Click here to return)
Klinger Thermoseal Miliam Mica PPS 150 Laminate
Categories: Ceramic; Oxide

Material Notes:
  • Type PSS
  • High Quality Mica Sheet
  • Laminated on Pegged Stainless Steel Insert
All Milam laminates are suitable for use in hot, dry gas applications such as exhaust manifolds, turbines, turbo chargers and air heat exchangers.

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Loss On Ignition <= 5.0 %DIN 52911
Thickness 1500 microns+/- 5% of nominal thickness
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1652 °F
 
Descriptive Properties
ColorMetallic Tan
Compressibility12-16 percentASTM F36A
Gas Permeability>100 ml/minDIN 3535/6
Pressure<14,503 psi
Recovery40-50 percentASTM F36A
Stress Relaxation4641 psi40 MPa/300°C, DIN 52913
 5801 psi50 MPa/300°C, DIN 52913
Tang Insert Stainless Steel Thickness0.004 inAISI 316

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Potassium Aluminosilicate (Muscovite Mica)
Crystex Composites Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 411 Moldable Glass-Mica Composite

PTHERM921 / 146075

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.