MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Total PSI 935E Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Polystyrene 935E is a high impact polystyrene exhibiting exceptional toughness for sheet and thermoforming applications.

This polymer is an excellent choice for cups, food packaging, custom sheet and coextrusion applications when extremely high ductility is crucial.

Information provided by Total Petrochemicals, Inc.

Key Words: Super high impact, toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 3.7 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2800 psiASTM D638
Elongation at Yield 60 %ASTM D638
Tensile Modulus 250000 psiASTM D638
Flexural Strength 5500 psiASTM D790
Flexural Modulus 260 ksiASTM D790
Izod Impact, Notched 2.50 ft-lb/inASTM D256
Falling Dart Impact 12.5 ft-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 198 °FHeat Distortion, Annealed; ASTM D648
Vicat Softening Point 208 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 80 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics STYRON® 484 High Impact Polystyrene
Americas Styrenics EA6740 High Impact Polystyrene
Ineos Nova 5400 High Impact Polystyrene
Total PSI 825E Polystyrene
A. Schulman Diamond TR 5000

PFIM919 / 38324

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.