MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Henkel Loctite® SpeedBonder™ 326 Fast Fixture Acrylic Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Acrylic Bonding Adhesives
Loctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond.

Bonding Type: Acrylic Typical Use: Fast fixturing applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Viscosity 18000 cPat 20 RPM
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 2700 psiVaries with substrates
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 225 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 min
 24.0 hourFull Cure
 
Descriptive Properties
ColorAmber
Gap Fill0.02 in.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil MED1-4855 Specialty Liquid Silicone Rubber - Unrestricted Medical Use
NuSil MED1-4213 Silicone, Two part Adhesive - Unrestricted Medical Use

PLOCT003 / 51739

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.