Description: PELLETHANE® 2355-55DE polyester polyadipate based polyurethane elastomer has excellent oil and chemical resistance. Applications include: Film, Sheet, Tubing, Recreation and sporting equipment, Industrial hoses, Fabric lamination, Sewer pipe linings, Footwear Data provided by Dow Chemical. |