MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ganpati Exim 1712 (SKS-30 ARKM-27) SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: The oil-filled styrene (alpha-methyl styrene)-butadiene SBR 1712 Rubber is produced by emulsion copolymerization of styrene and butadiene at 4-8 C, using as an emulsifier a mixture of disproprortionated liquid rosin, that is resinous and fatty acids of natural origin based. The technological process and methodics of production eliminate in synthesis processes using and formation of nitrose compounds. The diethylthydroxylamim is used in polymerization as a stopper. The polymer coagulates in a system “salt+acids” and does not contain any side inclusions of the structural and wet polymer. It is well mixing with different ingredients of rubber compounds and is easily treated on the simple rubber production equipment, is quite compatible with different rubbers of general use, has a low cost. In mixing with SBR 1500 at 1:1 rate the product will be of higher hardness, will grow tires abrasion resistance and will make bigger its running time up to 10%.

Application: The SBR1712 is general purpose rubber. It is widely used in tire, rubber technical, shoe, cable and other industries for production of automobile tires and tubes, wide assortment of rubber technical articles, white and colour shoes, cable castings and so on.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 47 - 57
@Temperature 100 °C
ML (1+4)
Deformation <= 20 %Residual Deformation After Break
Ash <= 0.60 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22 - 25 %Bound Styrene (Alpha-Methylstyrene)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength <= 22.0 MPa
Elongation at Break 550 - 750 %
Rebound <= 29 %Elasticity
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.00015 %
Iron, Fe <= 0.0040 %
 
Descriptive Properties
Content<0.15%Mass Fraction of Organic Acids Soaps
 0.0015Mass Fraction of Antioxidant, VS-1
 1.0-1.4%Mass Fraction of Antioxidant, VTS-150
 26-29%Mass Fraction of Oil
 4.0-5.6%Mass Fraction of Organic Acids
Mass losses at drying<0.35%
Viscosity Scattering0.05In one lot

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI023 / 317307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.