MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics M120F Mac-AS970W Aluminum silicate Ceramic
Categories: Ceramic; Oxide

Material Notes: It is typically a composite of 41.9% Al2O3 and 54.8% SiO2 with 2.3% TiO2, 0.75% Fe2O3 plus traces of MgO and CaO. By changing process conditions, this highly versatile material can be tailored to provide a range of hardness values to suit customer requirements, whilst maintaining its thermal and electrical properties. (See Rockwell hardness values to R15T, quoted alongside.)

Prime Features:

  • Excellent high temperature capability
  • Exceptional thermal shock resistance
  • Low and very stable thermal expansion
  • Hard and durable, with excellent resistance to abrasion and chemical attack
  • Can be precision formed into complex shapes that are not easily achieved with other materials
  • No special tooling required for forming
  • Good electrical properties
Typical Applications:
  • Thermally insulative components
  • Dicing support plates for wafer slicing
  • Furnace fixtures for glass sealing
  • Welding nozzles
Production Capabilities:
  • Precision machining in green state
  • Firing at precise temperatures to produce very close dimensional tolerances
  • Prototype, batch and volume production

Information provided by Morgan Advanced Materials

Key Words: M120F
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.30 g/ccfired
Open Porosity 2.0 - 3.0 %apparent, can be made impervious to water
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T <= 95nominal, tailorable range 50-95
Tensile Strength 17.6 MPa
Modulus of Elasticity 55.4 GPaYoung's
Flexural Strength 64.0 MPa
Compressive Strength 275 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 50000 ohm-cm
@Temperature 900 °C
 350000 ohm-cm
@Temperature 675 °C
 5.00e+6 ohm-cm
@Temperature 480 °C
 2.00e+9 ohm-cm
@Temperature 260 °C
 6.00e+11 ohm-cm
@Temperature 93.0 °C
 >= 1.00e+14 ohm-cm
@Temperature 24.0 °C
Dielectric Constant 5.3
@Frequency 1e+6 Hz,
Temperature 24.0 °C
Dielectric Strength 3.90 kV/mm
Dissipation Factor 0.010
@Frequency 1e+6 Hz,
Temperature 24.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.90 µm/m-°C
@Temperature 24.0 - 260 °C
 3.20 µm/m-°C
@Temperature 24.0 - 675 °C
 3.20 µm/m-°C
@Temperature 24.0 - 900 °C
Thermal Conductivity 1.26 W/m-K
@Temperature 300 °C
Maximum Service Temperature, Air <= 1150 °Cno load
Softening Point 1760 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 41.9 %
Fe2O3 0.75 %
SiO2 54.8 %
TiO2 2.3 %
 
Descriptive Properties
Colortan to pink
Te Value595 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum Silicate, Al2SiO5
Morgan Advanced Ceramics M120F Mac-AS970W Technical Ceramic
American Elements Titanium Nitride Nanoparticles
A-Glass Fiber, Generic
Morgan Advanced Ceramics AL 600™ Mac-A960W Aluminum Oxide Ceramic

CMORF5075 / 200313

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.