CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids intergranular corrosion, even on welded pieces without ulterior water quenching. Alloys CLC 18-10Ti exhibit austenitic microstructures free of deleterious carbide precipitations but with CNTi precipitations at the grain boundaries. The grade contains some residual ferrite (~ 4%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. The main properties are :- Basic corrosion resistance
- Resistance against intergranular corrosion
- Heat resistant alloy (medium temperature)
- High ductility
Information provided by manufacturer. |
EURONORM 1.4541 X6CrNiTi 18-10, AFNOR Z6 CNT 18-10, DIN W1.4541, ASTM A 240 – TP 321, UNS S32100 |