MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Skamol Group Skamol M-20 Insulating Mortar  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: SKAMOL insulating mortars have the following characteristics:
  • Max. service temperature: Up to 1150°C (2102°F)
  • Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grades in various applications
  • Good insulation values
  • Outstanding bonding properties within max. service temperature range
  • Water-retentive properties for quick and easy laying of dry bricks/blocks/slabs.
  • Combined air and heat-setting.

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 33.0 lb/ft³As Supplied
 56.0 lb/ft³Dried at 110°C (230°F)
Loss On Ignition 6.0 %
@Temperature 1025 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 900 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 11 %
CaO 1.0 %
Fe2O3 5.5 %
H2O, Water 2.0 %as supplied
K2O 1.3 %
MgO 1.0 %
Na2O 5.0 %
SiO2 67 %
TiO2 1.0 %
 
Descriptive Properties
Binder Silicate
Mixing Water Usage 22.5 liters to 25kg
Package Weight25 kgUnit weight, all included. Plastic sack with dry mix.
Pyrometric Cone Equivalent1040°CASTM C24-89, ORTON cones
Recommended Joint Thickness3.0-5.0 mm
Setting Mechanism air and heat-setting
Typedry mix
Usage 3 kgQuantity to fix 1m2 (11 ft2) of Slabs
 65 kgQuantity to set 1m3 (35.31 ft3) of Bricks

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSKAM027 / 2178

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.