MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® UltraPure 1292 MD Water Demineralization Resin
Categories: Polymer; Thermoset

Material Notes: For the demineralization of water in the production of ultra pure water (> 18MOhm*cm at 25°C) Lewatit® UltraPure 1292 MD is a ready-to-use mixed bed comprising a gel type strongly acidic cations exchange resin (SAC) and a gel type, strongly basic anion exchange resin (SBA, type I), individually with a monodispersed bead size distribution (uniform particles) based on a styrene-divinylbenzene copolymer for the use in working/regenerable and polishing/non-regenerable systems for the production of ultra pure water. The monodisperse beads (uniformity coefficient: max 1.1) are chemically and osmotically highly stable. The optimized kinetics lead to an increased operating capacity and the very low content of fines also results in a low pressure drop compared to ion exchange resins with heterodisperse bead size distribution. Lewatit UltraPure 1292 MD is correspondingly adjusted to the total capacity of the individual components to an equivalent ration of 1:1. In the regeneration step of a regenerable mixed bed, cation and anion exchange resins are clearly separated for providing a better quality of the service water. Lewatit UltraPure 1292 MD is highly regenerated and specially cleaned for meeting the specifications of the semiconductor industry. Leaching of organics from Lewatit UltraPure 1292 MD into the treated water is reduced to a level less than 10 ppb, and its resistivity achieves a level higher than 18 MOhm*cm.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.720 g/cc
Bead Size 0.580 - 0.680 mmMean, SAC
 0.590 - 0.690 mmMean, SBA
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 40.0 °C
 
Descriptive Properties
AppearanceBrown, translucent
pH Operating Range0 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8856 / 209248

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.