MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® 50 M44E Polyester Film, One-Sided PVDC Barrier Coated, 50 Gauge  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC) Coated Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

A transparent, exceptionally strong polyester film, coated on one side with an oxygen and moisture barrier PVDC copolymer. It is used as a substrate in combination with sealant webs, to produce a highly durable structure with excellent oxygen barrier. Can be printed with appropriate inks, including water based. The barrier coating may be adversely affected by certain solvents, if they are trapped during printing or laminating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccAverage value for Mylar® films.
Moisture Vapor Transmission 0.0800 cc-mm/m²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 6.00 g/m²/dayASTM E96 Procedure E
Oxygen Transmission 0.100 cc-mm/m²-24hr-atmor 6 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 0.500 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %ASTM D882
Film Elongation at Break, TD 80 %ASTM D882
Modulus of Elasticity 3.79 GPa(stiffness), ASTM D882
Tear Strength Test 350Graves, g; ASTM D1004
Film Tensile Strength at Break, MD 186 MPaASTM D882
Film Tensile Strength at Break, TD 228 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °CNot cleared by FDA for food temperatures above this temperature.
Shrinkage 1.4 %
@Temperature 150 °C,
Time 1800 sec
Film shrinkage in oven.
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %ASTM D1003
Gloss 200 %20°; ASTM D2457
Transmission, Visible 70 %% Clarity; ASTM D1746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Selar® PT 4274 Polyester Barrier Resin
Topaz, Al2SiO3(OH,F)2
Michelman® Topaz Indicator Solution

PDU664 / 33113

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.