Temper: 1/2 Hard Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding Common Fabrication Processes: Blanking; Forming and Bending; Heading and Upsetting; Shearing; Squeezing and Swaging Typical uses: Contacts; Electrical Connectors; Fuse Clips; Pole Line Hardware; Switch Parts; Fasteners; Washers; Diaphragms; Flexible Hose; Seamless Metal Hose; Strip Wound Hoses Applicable Specifications: Flexible Hose – ASTM B508; Wire – Trolly ASTM B9, ASTM B105 |