Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generation copolyester's most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Application/Uses - Extrusion blow molding
- Injection stretch blow molding
- Large refillable multi-use containers
Key Attributes - Ease of processing
- Excellent clarity
- Excellent hydrolytic stability
- Good chemical resistance
- Good heat resistance
- Outstanding impact resistance
|