MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nurel Engineering Polymers Promyde® B30 NC 100 PA 6, Dry, Heat stabilized, lubricated and Injection molded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Characteristics: Promyde B30 NC100 is a polyamide 6 heat stabilized, lubricated and nucleated for fast cycle injection molding. The incorporation of nano clay particles gives a product 20% stronger than conventional unfilled PA6, or PA66.

Applications: Promyde B30 NC100 provides significant weight reduction advantages over glass filled, glass bead filled, and mineral filled PA6, and PA66. Promyde B30 NC100 processes similarly to standard unfilled PA6 and can be used in PA66 moulds.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Moisture Absorption 2.30 %50%, rh; ISO 62
Water Absorption at Saturation 7.0 %in water; ISO 62
Viscosity Test 132 cm³/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0070 - 0.0085 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm
Melt Flow 145 g/10 min
@Load 5.00 kg,
Temperature 275 °C
[cm3/10 min], MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 100 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 4.0 %50 mm/min; ISO 527-1/-2
Elongation at Yield 3.5 %50 mm/min; ISO 527-1/-2
Tensile Modulus 4000 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 130 MPa2 mm/min; ISO 178
Flexural Modulus 3500 MPa2 mm/min; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.30 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
Melting Point 222 °CDSC 10°C/min; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1/-2
Flammability, UL94 V-2
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °Cinjection molding
Mold Temperature 40.0 - 80.0 °C
Drying Temperature <= 80.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 214 PPS, Unfilled
Lotte Advanced Materials Infino® XP-2130A PPS, 30% GF
Overview of materials for Thermoplastic Polyimide, Unfilled
Evonik VESTAKEEP® 1000P PEEK
DuPont Teijin Films Melinex® 054 Polyester Film

PNUREL011 / 183376

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.