MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound MX18001J Polypropylene, Unspecified (PP, Unspecified)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP STAT-KON MX18001J compound is based on Polypropylene (PP) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, Healthcare, Low Extractables.

Features: Low Extractable,Healthcare,Food Contact Acceptable,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Water Absorption <= 0.10 %
@Time 86400 sec
ISO 62-1
Moisture Absorption <= 0.100 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium <= 0.10 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation <= 0.10 %ISO 62-1
Linear Mold Shrinkage, Flow 0.013 - 0.017 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.011 - 0.015 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPa5 mm/min; ASTM D638
 30.0 MPa5 mm/min; ISO 527
Elongation at Break 1.7 %5 mm/min; ISO 527
 2.1 %5 mm/min; ASTM D638
Tensile Modulus 2700 MPa1 mm/min; ISO 527
 2950 MPa5 mm/min; ASTM D638
Flexural Strength 54.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 55.0 MPa2 mm/min; ISO 178
Flexural Modulus 2600 MPa2 mm/min; ISO 178
 2750 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 10.0 JASTM D256
Izod Impact, Unnotched 250 J/mASTM D4812
Izod Impact, Notched (ISO) 1.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 10000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 79.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
ASTM E831
 100 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 86.0 µm/m-°C
@Temperature -40.0 - 60.0 °C
ASTM E831
 110 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 121 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 122 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 70.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 240 - 250 °C
Melt Temperature 225 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81327 / 289274

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.