MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi PPX Polypropylene Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: A specially modified PP to print well with any printer. This material is great for non-abrasive fixturing, living hinges, covers, and general-purpose material.

Features:

  • Good flexibility
  • Excellent impact resistance
  • Good layer adhesion
Colors: PPX is available in Black

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.890 g/ccISO 1183
Filament Diameter 1750 µmTolerance: 50 µm, =95% Roundness
Melt Flow 14 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12.7 MPaISO 527
Tensile Strength, Yield 12.6 MPaISO 527
Elongation at Break 5.0 %Strain at Break; ISO 527
 <= 450 %ISO 527
Elongation at Yield 33 %ISO 527
Flexural Modulus 424 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 - 260 °CISO 527
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 260 °C
 
Descriptive Properties
Bed Temp75-100°C
Nozzle diameter=0.4mm
Print Speed30-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9844 / 301069

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.