MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Coating P. Materials CS-688SH TPU for Shoe Adhesion
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Solvent-based TPU hot-melt adhesive. It can be dissolved in MEK, Acetone, EAC, etc., used as PU adhesives. And has many characteristics like below: Excellent green bonding strength; Fast dissolution rate; High speed of crystallization; Individually using, or with cross linking agents. Products are used in lamination for shoes/ textile products, fire hoses (extrusion), furnishing (MDF boards) lamination, and TPU, PVC, Nylon, fabrics & leather lamination.

Product Description: Solvent-based TPU hot-melt adhesive, can be dissolved in MEK, Acetone, EAC, etc.

Application To End-Use Products: Products are used in lamination for shoe/ textile products, fire hoses (extrusion)

Information provided by Coating P. Materials Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 3300 - 4200 cP
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 1.57 - 2.16 MPaPVC vs. PVC after 10 Mins
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 - 12.0 minTack Time, PVC vs. PVC
 
Descriptive Properties
Activation Temperature55-65°C
Crystallization Rate16-22 min
Heat Resistance?3 mm70?, PVC vs. PVC
Toluene in Solvents15-20%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTCOAT139 / 294083

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.